Over time, very fine whiskers of pure metal can form on
electroplated zinc, cadmium, or tin surfaces. If these whiskers
are disturbed, they may break off and become airborne, possibly
causing failures or operational interruptions. For over 50 years,
the electronics industry has been aware of the relatively rare,
but possible, threat posed by metallic particulate contamination.
During recent years, a growing concern has developed in
computer rooms where these conductive contaminants are
formed on the bottom of some raised floor tiles.
Although this problem is relatively rare, it may be an issue
within your computer room. Since metallic contamination can
cause permanent or intermittent failures on your electronic
equipment, Hewlett-Packard strongly recommends that your site
be evaluated for metallic particulate contamination before
installation of electronic equipment.